The authors of the neodymium plating paper wrote back.. looks to be about $20,000 of investigation
the substrate has to smooth
Titanium coated Si wafer??
Sputtering might be quicker..
Finally, the AFM investigation of the targets showed
that smooth layers can be grown ONLY using smooth
deposition substrates. Moreover, the MP production of
smooth and crack-free layers proved to be possible ONLY
when smooth substrates like Ti-coated Si wafer, and lowvolatility
plating solvents like DMF are used.